L360 pipeline chalybe consuetudo processui pipeline transport pipe
L360 Pipeline Steel, Propositum: API SPEC 5L-2011 (Pipeline Specification), enucleata et divulgata ab Instituto Americano Petroleo, per orbem terrarum adhibetur.Pipepipe: Ad transportandum oleum, gas vel aquam de terra per pipepipes ad oleum et gas industriam.Fistula piperis inconsutilis et iuncta duo genera habet, tibia finem habet finem planum, finem lina et nervum;Connexio modus est finis glutino, upupa connexio, nexus nervus et caetera.Summa materia tubi est B, X42, X46, X56, X65, X70, et alia gradus ferri.Societas nostra cum API certificatione (API 5CT et API 5L) mense Augusto 2009 transiit.
L360 Pipeline Steel, API SPEC 5L GB/T9711.1 GB/T9711.2 China National Latin Application: Oxygen, aqua et oleum tibiae partus in oleo et industria gasi B, X42, X52, X60, X65, X70 L245 L290 L320 L360 L390 L450 L485
Cum evolutione technologiae laminarum pipelinearum et progressum fistulae iunctae formantis, technologiae glutino, applicationis fistulae cum fistula iuncta gradatim expandendo, praesertim in magna diametri fistulae genere scopo iuncta commoda magis apparentia et factores sumptus; iuncta fistula dominatus est in campo fistulae lineae, quae evolutionem ferro incorruptam sesutilem ferro recta fistula terminat.Anno 2004, output fistulae inconsutilis circiter 40 000 t sunt, gradus chalybis X42-70 includit, et varietates pipelineorum et fistulae subaquaneae sunt.
Productio alti ferrei gradus pipelinei fistulae microalloying calefactionis processum curationis adhibet, productio sumptus fistulae immaculatae ferro inconsutilis, altior patet quam fistula iuncta, et cum emendatione gradus ferri, ut X80 et supra, gradus fistulae pipelines ferro in aequivalenti carboni limite. processus conventionalis inconsutilis fistulae difficilis occurrit requisitis utentium;Quaelibet 12Cr1moV fabrica fistula mixturae opus investigationis scientificae exercet ad resistentiam fistulae pipelineae et stabilis effectus in environment humilis et caliditas.
L360 Pipeline Steel, The Material
L245, L360, A53, J55, N80, X42, X46, X52, X56, X60, X65, X70;
L360 Pipeline Steel, Specifications
∮60-630×1.53-40
L360 Pipeline Steel, Mechanica Properties
vexillum | notam | Roboris distrahentes -MPa) | Mpa) | ostendit | elongatio% | 0 impulsum navitas Akv (J)
| Calor curatio conditio |
API SPEC 5L GB/T9711.2 | B | ≥415 | 245~440 | ≤0.80 | 22 | ≥40 | Estne ignis |
X42 | ≥415 | 290~440 | ≤0.80 | 21 | ≥40 | Estne ignis | |
X52 | ≥460 | 360~510 | ≤0.85 | 20 | ≥40 | Estne ignis | |
X60 | ≥520 | 415~565 | ≤0.85 | 18 | ≥40 | Estne ignis | |
X65 | ≥535 | 450~570 | ≤0.90 | 18 | ≥40 | restinguere + temperare | |
X70 | ≥570 | 485~605 | ≤0.90 | 18 | ≥40 | restinguere + temperare |
L360 Pipeline Steel, Chemical Composition
vexillum | notam | Chemica compositio (%) | CEV(%) | |||||||
C | Si | Mn | P | S | V | Nb | Ti | |||
API SPEC 5L GB/T9711.2 | B | ≤0.16 | ≤0.40 | ≤1.10 | ≤0.020 | ≤0.010 | . | . | . | ≤0.42 |
X42 | ≤0.17 | ≤0.40 | ≤1.20 | ≤0.020 | ≤0.010 | ≤0.05 | ≤0.05 | ≤0.04 | ≤0.42 | |
X52 | ≤0.20 | ≤0.45 | ≤1.60 | ≤0.020 | ≤0.010 | ≤0.10 | ≤0.05 | ≤0.04 | ≤0.45 | |
X60 | ≤0.21 | ≤0.45 | ≤1.60 | ≤0.020 | ≤0.010 | ≤0.15 | ≤0.05 | ≤0.04 | ||
X65 | ≤0.16 | ≤0.45 | ≤1.60 | ≤0.020 | ≤0.010 | ≤0.06 | ≤0.05 | ≤0.06 | ≤0.45 | |
X70 | ≤0.16 | ≤0.45 | ≤1.70 | ≤0.020 | ≤0.010 | ≤0.06 | ≤0.05 | ≤0.06 | ≤0.45 |
Nota:1.0.015% ≤Altot< 0.06%;N 0,012% vel minus;Al/N 2/1 vel superior;Cu 0,25% vel minus.Ni 0,30% vel minus.Cr 0,30% vel minus;Mo≤0.10% 2.V +Nb+Ti≤0.15 3.X60, X65, X70 Ut constat Mo≤0.35% API SPEC 5L